Builder › Guides › DTF heat press settings

DTF heat press settings

Typical starting points for pressing DTF transfers. Films and powders differ, so your supplier's instructions always win. When in doubt, test on a scrap first.

Settings by fabric

FabricTemperatureTimePressure
Cotton300 to 320 °F · 150 to 160 °C10 to 15 sMedium to firm
Cotton and polyester blends290 to 310 °F · 145 to 155 °C10 to 15 sMedium to firm
Polyester260 to 285 °F · 125 to 140 °C8 to 12 sMedium
Nylon, performance wear250 to 275 °F · 120 to 135 °C8 to 10 sLight to medium
Canvas, denim, tote bags300 to 320 °F · 150 to 160 °C12 to 15 sFirm

These are common ranges, not a guarantee. Low-temperature films exist that press well below these numbers. Check the instructions that came with your transfers.

The pressing steps

  1. Pre-press the garment for 3 to 5 seconds. This removes moisture and flattens wrinkles and seams.
  2. Place the transfer with the printed side down, film on top. Cover with parchment paper or a Teflon sheet if your press plate is not clean.
  3. Press at the temperature, time and pressure for your fabric.
  4. Peel as your film requires. Cold peel film must cool completely first. Hot peel film is peeled straight away. Peel low and slow, in one smooth motion.
  5. Press again for 5 to 10 seconds with parchment or a Teflon sheet over the design. The second press pushes the ink into the fibres, improves wash life and takes away some shine.

Hot peel or cold peel?

Hot peelCold peel
When to peelRight after pressingAfter it has cooled to room temperature
SpeedFaster for productionSlower
FinishUsually a little glossierUsually more matte
Forgiving?Less. Peeling too late can lift edges.More. Peeling too early is the main mistake.

If you do not know which film you have, treat it as cold peel. A cold peel film peeled hot is ruined. A hot peel film peeled cold is usually fine.

Fixing common problems

ProblemLikely causeTry
Edges lift when peelingToo little pressure or heat, or peeled at the wrong timeMore pressure, 5 more seconds, check hot or cold peel
Design cracks after washingUnder-pressed, or no second pressAdd the second press, raise pressure
Shiny box around the designPress marks from heat and pressure on the fabricLower the temperature, use a pressing pillow, press only the design area
Colours look dull or the shirt colour shows through on polyesterDye migration from too much heatLower the temperature, shorten the time
Scorch marks or yellowingToo hot or too longLower the temperature, cover with parchment
Thin lines or small text do not transferDetail is too fine to hold adhesiveThicken lines to at least 0.5 mm in the artwork

Washing

  • Wait 24 hours before the first wash.
  • Wash inside out in cold or warm water.
  • Tumble dry low or hang dry. Do not iron directly on the design.

Need transfers? Lay out your gang sheet for free.

Open the builder